Welcome to Guangzhou Wellcare Silicone Products Co., Ltd. official website!
  • Scan for Mobile Store
    Scan QR code to access mobile store
Guangzhou Wellcare Silicone Products Co., Ltd.

Liquid silicone molding, clean-room assembly, charging module integration


Platinum Silicone Personal Wellness Component LSR Molding OEM

Price¥1.45

MOQ1000 pieceStock:0 piece

Delivery Time
30 days
Location
China Jiangsu Suzhou
Valid Until
Long-term
Updated
2026-10-19 22:27
Views
23

Company Card

  • CompanyGuangzhou Wellcare Silicone Products Co., Ltd.
  • Contact (Mr.)
  • AddressPanyu District, Guangzhou, Guangdong, China

Buyers Also Viewed

Product Details
Material:
Platinum-cured LSR, phthalate free
Hardness Range:
10 to 60 Shore A
Process:
LSR injection, clean-room assembly

Body-contact silicone parts are specified by their material, not by their shape, and the material is decided by the cure system. Platinum-cured liquid silicone rubber gives a low-volatile product with predictable compression set, which is why it is the default for any part intended for prolonged skin contact.

We mould LSR components in Guangzhou for wellness device brands and private-label programmes, with assembly carried out in a controlled area separate from the moulding floor.

Why platinum cure

Peroxide-cured silicone is cheaper but leaves peroxide by-products in the part, and those by-products are what shows up as an odour in a sealed retail pack. Platinum cure avoids that, holds compression set better across a temperature range, and can be pigment-matched with a tighter tolerance because the catalyst is not consumed by the pigment carrier. For body-contact parts the difference is visible in the odour test and in the aging behaviour.

Specification

MaterialPlatinum-cured LSR, translucent or pigmented
Hardness10 to 60 Shore A, 5 A steps
Colour toleranceDelta E under 1.0 against a supplied standard
Wall thickness0.6 mm minimum on 1:1 moulding, 1.2 mm recommended
Temperature-40 to 200 C service range
AssemblyClean-room area with glove and hygiene protocol
MOQ1,000 pieces per SKU

Tooling for LSR

LSR runs at a low viscosity and a high temperature on a cold runner system, and it flashes easily, so parting lines have to be designed rather than accepted. Cold deck runners add tooling cost but cut scrap to near zero on parts with a visible parting line. Where a part has an undercut, we prefer a sliding insert over a collapsible core, because LSR will tear before it collapses.

Surface finish

A high gloss finish is achievable but is rarely the right choice for a body-contact part: it retains fingerprints and shows every blemish on a moulded surface. Matte finishes, applied by blasting the tool cavity, hide minor imperfections and reduce surface friction, which matters on a part that is handled repeatedly.

Testing and documentation

Compression set is measured at 22 hours and at 70 C. Tear strength is checked on the same lot as production. Material declarations cover BPA, phthalates, heavy metals and latex, and any product-level testing is carried out by a laboratory appointed by the buyer. We supply declarations for our material; we do not issue certificates in another company's brand name.

Commercial notes

Copy, photography and packaging for this category are kept to a discreet, non-explicit standard that suits mainstream marketplaces and general retail. We will not produce mouldings from artwork or drawings that reference a protected design without the buyer holding the rights.